| Serial number | Project | Detail |
| 1 | Camera light source | HD line scan camera; Line laser |
| 2 | Size |
1.Specific combination of actual layout scheme design 2.Automatic blanking is provided |
| 3 | Capacity | >4000 |
| 4 | Support cell |
1. Single crystal 2. 156-230mm |
| 5 | Cell state | Finished battery piece shoot the front of the battery piece |
| 6 | Shooting defect |
PL can be photographed defects: black spots suction cup marks graphite boats hidden cracks etching oil spots concentric circles scratches Other pollution and all the usual defects(★Different battery processes will lead to differences in the strength of defect imaging) |
| 7 | Process contribution |
1.AI algorithm automatically detects 2.Hidden crack culling alarm to prevent batch defects 3.Break grid virtual printing alarm prevent batch defects |
| 8 | Advantage |
1.Contactless loss 2.Probe free loss 3.High productivity 4.SE offset off grid virtual printing poor sintering appear white more obvious than EL |